Project | INV-V650 |
Appearance (visual inspection) | white cloudy liquid |
Viscosity (mPa.s) | 200-300 |
Density (g/cm3, 25ºC) | 1.1-1.2 |
Storage temperature (ºC) | normal temperature |
Suggested recipe | Name | Weight ratio | |
INV-V650 | 100 | ||
Hardener AKZO M-50 | 1-2 | ||
Accelerator AKZO NL 49P(1% Co) | 0.5-2 | ||
The recommended weighing tool is accurate to 0.5% to ensure the accuracy of the ratio; first add the accelerator and stir it evenly, then add the curing agent and stir it evenly before use, and cannot be added at the same time. | |||
If too much resin is mixed at one time, the pot life of the product will be shortened; | |||
Gel time | Temperature (ºC) | Gel time (min) | |
25 | 30-60 | ||
The gel time can be adjusted by the amount of accelerator added, and the product can be adjusted according to customer needs after it exceeds the range. |
Test items | Typical value | Unit |
Oxygen Index | 45 | |
Tensile Strength | 480 | MPa |
Bending strength | 510 | MPa |
Bending strength after boiling for 2h | 420 | MPa |
Item No. | Gel Time(25ºC)Min | Chemical Category | Features | Application |
INV-V411 | 10-17 | Bisphenol A | Excellent construction technology; excellent corrosion resistance, good corrosion resistance to general acids, alkalis, salts and organic solvents; high solid content, excellent mechanical and mechanical properties | Chemical anti-corrosion equipment, engineering, sporting goods, transportation. |
INV-V411M | 8-18 | Bisphenol A | Standard bisphenol A type epoxy vinyl ester resin. Excellent construction technology, excellent corrosion resistance | Widely used in chemical engineering of many chemical media such as acid, alkali, salt, organic solvent and pipes, tanks, towers, tanks, pools in industry. |
INV-V411W | 20-30 | Bisphenol A | Excellent corrosion resistance, combined with performance and cost advantages, with better price/performance ratio | Anticorrosion equipment and engineering in conventional chemical industry. |
INV-V411L- GXX | 30-120( can be customized) | Bisphenol A | Has lower viscosity, adjustable gel time, lower exothermic peak | Vacuum infusion molding process to prepare composite products, such as boats, wind power fields |
INV-V416 | 8-14 | High reactivity, heat resistance, excellent toughness | Rapid pultrusion to prepare rods, cores, pipes and other products | |
INV-V440 | 15-55 | Low cure shrinkage, pre-acceleration, anti-sag | Preparation of composite molds, or composite products with low shrinkage requirements | |
INV-V480 | ---- | Mgo Thickening | High reactivity, thickening with magnesium oxide | SMC molding process to prepare battery shells, fan impellers, etc. |
INV-V495 | ---- | Mgo Thickening | High toughness, magnesia thickener | Used together with low shrinkage agent, it can prepare products with low shrinkage, high strength, high toughness, high heat resistance and heat aging resistance, etc. It is suitable for BMC, SMC, prepreg and other molded products. e.g. composite toe caps, helmets. |
INV-V650 | 30-60(can be adjusted based on the accelerator content) | Halogen Free Flame Retardant | Halogen-free, in addition to the corrosion resistance of conventional epoxy vinyl ester resins, it also has good flame retardancy. It is an integrated solution product with anti-corrosion and flame retardant properties. | Mainly used in corrosion-resistant equipment with flame retardant requirements, such as wet electrostatic precipitators in thermal power plants, chimneys, etc. |
INV-V470 | 10-30 | Phenolic Aldehyde | Phenolic modified epoxy vinyl ester resin, high crosslinking density, HDT=145 ºC, has more excellent heat resistance and corrosion resistance; especially in acid oxidizing environment, it has long-term resistance. | Heavy-duty anti-corrosion fields with strong corrosiveness and high temperature in chemical engineering and industry. |